21 Nov 2009 
Support Center » Knowledgebase » What are the optimum PH for your anodizing dyes?
 What are the optimum PH for your anodizing dyes?
Solution

DYES

OPTIMUM Ph

RED BORDEAUX

6

YELLOW 4A

6

BLUE 4 A

6

VIOLET 3D

6

BLACK HBL

5.5

GREEN SCG

6.6

GOLD S

6

TURQUOISE

5.5

OLIVE DRAB

7.5

GOLDEN ORANGE

7

GREY BL

5.5

BROWN GL

6.5

TEAL

5.5

ELECTRIC BLUE

6

COPPER BF

7

FLOURESCENT PINK

BRONZE

5.5

DEEP RED

5.5

FLOURESCENT YELLOW

6

GREEN AEN

6

VIOLET DS

6

GREY NLN

5.5

YELLOW 3GL

6

BROWN BL

6.5

FAST BLUE

5.5

ORANGE 3A

6



Article Details
Article ID: 58
Created On: 17 Aug 2005 05:23 PM

 This answer was helpful  This answer was not helpful

 Back
 Login  
Username:
Password:
Remember Me:
 
 Search
 Article Options
Home | Submit a Ticket | Knowledgebase | Troubleshooter | News | Downloads | Customer Forum | Videos & Tutorials | Contact Us | Radio Controlled Model Support
Language:

Help Desk Software By Kayako SupportSuite v3.60.04