How much will the Plug N' Plate solutions plate? At an average thickness the kits will plate approximately: 4oz Gold - 0.5 - 1 sq ft 4oz Silver - 1 sq ft 8oz Nickel - 2 sq ft 8oz Copper - 2 sq ft 8oz Copy Chrome - 2 sq ft 8oz Bronze - 2 sq ft 8oz Tin - 2 sq ft 4oz Brass - 1 sq ft Choose files or drag and drop files Tags: Was this article helpful? Yes No Lance Caswell Posted TweetShare on Facebook Comments Please sign in to comment