DYES
OPTIMUM Ph
RED BORDEAUX
6
YELLOW 4A
6
BLUE 4 A
6
VIOLET 3D
6
BLACK HBL
5.5
GREEN SCG
6.6
GOLD S
6
TURQUOISE
5.5
OLIVE DRAB
7.5
GOLDEN ORANGE
7
GREY BL
5.5
BROWN GL
6.5
TEAL
5.5
ELECTRIC BLUE
6
COPPER BF
7
FLOURESCENT PINK

BRONZE
5.5
DEEP RED
5.5
FLOURESCENT YELLOW
6
GREEN AEN
6
VIOLET DS
6
GREY NLN
5.5
YELLOW 3GL
6
BROWN BL
6.5
FAST BLUE
5.5
ORANGE 3A
6