Can I Store The Kit Without The Solution Going Bad?
Posted by Lance Caswell on 14 August 2005 04:34 PM

Yes. You can put the kit aside for as long as you like. Just remove the anodes and securely attach the locking lid. We recommend transferring the chrome solution into a glass container. The acid very slowly dissolves the plastic tank.

After a long storage, it may be necessary to add some brightener back into your system to begin plating.