DYES

OPTIMUM Ph

RED BORDEAUX

6

YELLOW 4A

6

BLUE 4 A

6

VIOLET 3D

6

BLACK HBL

5.5

GREEN SCG

6.6

GOLD S

6

TURQUOISE

5.5

OLIVE DRAB

7.5

GOLDEN ORANGE

7

GREY BL

5.5

BROWN GL

6.5

TEAL

5.5

ELECTRIC BLUE

6

COPPER BF

7

FLOURESCENT PINK

BRONZE

5.5

DEEP RED

5.5

FLOURESCENT YELLOW

6

GREEN AEN

6

VIOLET DS

6

GREY NLN

5.5

YELLOW 3GL

6

BROWN BL

6.5

FAST BLUE

5.5

ORANGE 3A

6