You polish magnesium using the same procedure as polishing aluminum. Our Aluminum Polishing Kit [http://www.caswellplating.com/aluminum-copper-alloy-polishing-kit.html] will work for this, and is especially useful for wheels. Because magnesium is slightl...
Use our White Lightning Compound [http://www.caswellplating.com/white-lightning-stainless-rouge-c-170.html] (F515-6113) with a spiral sewn or loose cotton wheel. If desired, you may finish with the Blue Compound [http://www.caswellplating.com/blue-buffin...
To remove scratches and haze in these materials, use our White Lightning compound [http://www.caswellplating.com/white-lightning-stainless-rouge-c-170.html] (F515-6113) and a spiral sewn cotton wheel. For faster polishing, you could use our Excello bu...
We recommend an application of Glu-Tite before the greaseless compound, to improve adhesion to the buffing wheel.Turn your buffing machine on, get it up to full speed then turn it off. As soon as you turn it off, hold the stick of Glue-Tite against the wh...