Airbrush Kit Instructions

Airbrush Kit Instructions

                                   AIR-BRUSH KIT
                                 HOW TO AIR-BRUSH
                                 INSTRUCTION BOOK

MIXING PAINT
You can custom mix any color combination you wish. REMEMBER: Paints must be
compatible… that is, mix enamels with enamels, lacquer, etc. Mix thoroughly. Make
sure paint is free of lumps…strain if necessary.

THINNING
Most jar paints are too heavy to spray. Enamels should be thinned approximately 1 part
paint to 1 part thinner. To thin automotive lacquers, consult the spraying directions on
the other side of the paint container.

WHEN USING LACQUER
Lacquer dries very quickly. For best results the operation should be continuous, that is,
the air brush should not be set down for more than a few moments before resuming spray.
Keep an extra paint jar of thinner handy…remove lacquer jar, attach jar of thinner and
spray to clean out any lacquer that may dry in air brush. Also refer to cleaning
instructions for additional information.

COMPONENT PARTS
AIR TIP FINE                   PLUNGER SPRING                 PAINT JAR W/ CPVER
AIR TIP-BRUSHING               AIR HOSE FITTING               COUPLING NUT
PLUNGER HEAD                   PROPEL REGULATOR               5 FT. AIR HOSE
                               VALVE
AIR TIP-SEAL                   WRENCH                         PAINT SEAL
HANDLE                         350 JAR ADAPTOR FOR            COMPLETE ASSEMBLY
                               ¾ oz AND 2 oz JAR
SPACER                         JAR COVER GASKET               LOCK NUT
O RING x 3                     SYPHON TUBE                    FLUID NEEDLE FINE
PLUNGER                        ¾ oz PAINT JAR W/
                               COVER

TO ATTACH
1. Attach air-regulator to air-hose.
2. Attach air-regulator to propel can.
3. Attach other end of air-hose to air-brush by turning in a clock wise motion on a fitting.

TO TURN ON AIR
1. Turn knob clock wise to desired pressure.
2. For less pressure or to turn off, turn knob in counter clock wise direction.
Then air regulator valve is designed for propellant cans. It will adjust pressure from 45 to
50 PSI. For large jobs and prolonged spraying a compressor of CO2 tank is
recommended. When air is regulated pressure should be between 45 to 50 PSI. Normal
operating pressure is 30 PSI.
TO OPERATE
After mixing and thinning paint, tilt paint jar about 2/3 full (or less). Attach jar of paint
to air brush, turn air on and press trigger. Test your spray on old newspaper or other
materials; make any necessary spray adjustments, and get the “feel” of your brush. (Be
sure that paint of fumes cannot reach any flame. Also make sure that there is adequate
ventilation.)

ADJUSTING PAINT FLOW
Paint flow and spray pattern are adjusted by turning the fluid cap (see illustration) at front
of air-brush. Fluid cap is completely closed when it has been turned clock wise to stop
point. Using thumb and index finger turn fluid cap counter clockwise to obtain various
degrees of paint flow. Maximum flow will be attained by turning fluid cap
approximately 4 half turns counter clock wise.

PAINT MISCELLANEOUS
Do blow test using old newspaper when changing paint illustration (actual object) station
nozzle’s position, air strength and distance. Remember the condition of mist.
A: 00 (Degrees) Adjustment dial rotation angles
B: Air strength & storing, medium, weak
C: 00mm Nozzle and paint surface distance.
Prepare object to be painted, masking off any area that should not be painted. (Be sure
object is clean and free of dust, grease, etc.) Small objects such as models, etc. should be
hung or placed on a pedestal so all areas to be sprayed, can be easily reached. (A stand
may fashioned from an ordinary wire cost hanger, or bottle, etc.) Hold nozzle of air
brush about 6 inches from surface. Use short strokes moving air brush constantly at a
steady rate, parallel to the surface. Don’t spray too heavy, rather, apply a light coat, let
dry then another coat, let dry, etc, until desired coverage is achieved.

LEARN TO TRIGGER
Best results are achieved by a good constant motion. Start motion before pressing
trigger, follow through motion after releasing trigger.
If air brush motion is uneven, paint finish will be uneven.

THE MOST COMMON PROBLEM
Runs and sags are caused by one or more of the following errors.
1. “Freezing” or forgetting to release trigger at end of spray.
2. Holding air-brush still or moving too slowly.
3. Holding air-brush too close to surface.

For best results always clean immediately after using. Remove and empty paint jar.
Wipe thoroughly including inside of cover. Fill jar ½ full of thinner and reattach to air-
brush. Spray up fluid cap with soft cloth and force air and thinner back and forth thru
needle, cap and tip.
Should air-brush become clogged, remove needle, cap and tip using the following
procedure hold fluid cap and locknut using thumb and index finger. Place wrench
(provide in kit) on a flat surface of fluid needle and turn counter clock wise. Fluid
needles can then be easily taken out.

TECHNIQUES TO USE
Masking of frisket is used mostly when more than one color is appeared. A new frisket is
out for each color and covering any area that should not be sprayed. Frisket paper is
available at our supplies store.
A flat surface mask can cut from acetate or stiff paper. For a sharp edge, hold mask flat
in position. For edge, elevate the mask lightly by resting on ruler or other flat object.
For contour masking (models, ceramic, etc.) use masking tape, scotch tape, or out to
desired shape, make sure edges are pressed firmly against surface. In addition, office
supply stores carry. Avery pressure sensitive labels. These labels make excellent masks.

Clean needle, fluid cap and air tip with a small piece of cotton dipped to thinner. To
reassemble reverse above procedure.
When using quick drying paint. It is advisable to clean of immense fluid end of brush in
a compatible solvent between sprays.

STENCILS
Stencils are used when a design needs to be duplicate, ideal for patterns and decorating.
Out it from hard paper, hold firmly to position and spray start with edges and with
inward. A reverse stencil also be used, spray along stencil edge.