Aluminum & Copper Polishing Kit

Aluminum & Copper Polishing Kit

                                 1.     For best results, thoroughly clean part to remove all
                                        grease and dirt
                                 2.     File or Emery paper all deep marks and scratches
                                 3.     Use the Sisal wheel (ropelike) and the black emery bar
                                        to buff the entire area. Use the cone bob and the black
7696 Route 31, Lyons, NY 14489          compound to get into diffcult areas.
         855-CASWELL             4.     Apply small quantities of compound to the wheel
                                        frequently
       caswellplating.com
                                 5.     Use the Spiral Sewn wheel and the brown compound to
   sales@caswellplating.com
                                        finally bring a high shine to the workpiece
                                 6.     Use the Loose Cotton wheel to get into difficult areas
                                        with the brown compound
                                 7.     Use the white liquid rouge and follow instructions on
ALUMINUM & COPPER                       the label
  ALLOY BUFFING &                     Wheels should be fitted to a fast electric drill or air tool
   POLISHING KIT
                                 For help using this product, access our free Polishing Forum
                                              at http://forum.caswellplating.com




                                        1.    For best results, thoroughly clean part to remove
                                              all grease and dirt
                                        2.    File or Emery paper all deep marks and scratches
                                        3.    Use the Sisal wheel (ropelike) and the black emery
                                              bar to buff the entire area. Use the cone bob and
7696 Route 31, Lyons, NY 14489                the black compound to get into diffcult areas.
        855-CASWELL                     4.    Apply small quantities of compound to the wheel
                                              frequently
      caswellplating.com
                                        5.    Use the Spiral Sewn wheel and the brown
   sales@caswellplating.com
                                              compound to finally bring a high shine to the
                                              workpiece
                                        6.    Use the Loose Cotton wheel to get into difficult
                                              areas with the brown compound
ALUMINUM & COPPER                       7.    Use the white liquid rouge and follow instructions
  ALLOY BUFFING &                             on the label

   POLISHING KIT                      Wheels should be fitted to a fast electric drill or air tool

                                 For help using this product, access our free Polishing Forum
                                              at http://forum.caswellplating.com

    • Related Articles

    • Plug N Plate® Kit Instructions

      Plug N’ Plate® Brush Plating System I am a watchmaker in Scottsdale, Arizona and I specialize in restorations of fine antique watches and clocks. I was recently commissioned to restore a one-of-a-kind French clock, Circa. 1860 which was ornamented ...
    • What products do you recommend for polishing magnesium?

      You polish magnesium using the same procedure as polishing aluminum. Our Aluminum Polishing Kit will work for this, and is especially useful for wheels. Because magnesium is slightly softer than aluminum, you may want to use the Spiral Sewn or Loose ...
    • SCIENCE KIT ZINC

      CASWELL SCIENCE PLATING KITS ZINC PLATING Electroplating is a process that uses electricity to move metallic ions from a metal containing solution onto another surface. The process was invented in the early 1800’s and while the specific techniques ...
    • Electroless Copper Kit Instructions

      Instructions For Plating With Our Electroless Copper system, including plating PCB Thru-Holes.
    • Aluminum Blackener

      CASWELL INC Safety Data Sheet Aluminum Blackener SECTION 1: Identification 1.1 Product identifier Product name Aluminum Blackener Product number A385 Brand CASWELL 1.3 Recommended use of the chemical and restrictions on use Metal Blackening of ...