Can I Use Your Kits To Plate Aluminum?
Yes! Using our Zincate Concentrate, the parts are pre-treated and can then be plated in our plating kits. For best results, plate Zincated items in Flash Copper first.
Related Articles
Plug N Plate® Kit Instructions
Plug N’ Plate® Brush Plating System I am a watchmaker in Scottsdale, Arizona and I specialize in restorations of fine antique watches and clocks. I was recently commissioned to restore a one-of-a-kind French clock, Circa. 1860 which was ornamented ...
Can I Use Your Kits To Plate Lead?
Yes. You must dip in Pickle #4, then pre-plate the parts with Flash Copper prior to plating with any other kit.
Changes To Electroless Kits
IMPORTANT CHANGES TO INSTRUCTIONS FOR ELECTROLESS NICKEL, KROME, COBALT AND BORON NITRIDE PLATING INSTRUCTIONS Instead of the ceramic heaters mentioned in the plating manual, we now supply glass lined tanks and a thermometer with these kits. The ...
Can I use your kits to plate Pot Metal or Zinc Die Cast?
Yes. You must pre-plate the parts with Flash Copper prior to plating with any other kit.
How Long Will My Plate Last?
That depends on how long you plate your part for. The longer you plate it, the longer the plate will last. All our plating kits use the same chemicals and processes as the plating shops that plated your parts originally. You can expect the same or ...