Can I use your kits to plate Pot Metal or Zinc Die Cast?
Yes. You must pre-plate the parts with Flash Copper prior to plating with any other kit.
Related Articles
Can I Use Your Kits To Plate Aluminum?
Yes! Using our Zincate Concentrate, the parts are pre-treated and can then be plated in our plating kits. For best results, plate Zincated items in Flash Copper first.
SCIENCE KIT ZINC
CASWELL SCIENCE PLATING KITS ZINC PLATING Electroplating is a process that uses electricity to move metallic ions from a metal containing solution onto another surface. The process was invented in the early 1800’s and while the specific techniques ...
Plug N Plate® Kit Instructions
Plug N’ Plate® Brush Plating System I am a watchmaker in Scottsdale, Arizona and I specialize in restorations of fine antique watches and clocks. I was recently commissioned to restore a one-of-a-kind French clock, Circa. 1860 which was ornamented ...
My Plug N Plate Kit Doesn't Plate
If your Plug N Plate® kit doesn't plate, check the following things: Check your connections are correct and tight. The black alligator clip should be on the part being plated, and the wand should be on the red banana plug and tight. Check the bandage ...
Plug N Plate Zinc MSDS
CASWELL INC Safety Data Sheet Plug N Plate Zinc Solution SECTION 1: Identification 1.1 Product identifier Product name Plug N Plate Zinc Solution Product number PNPZN Brand Caswell 1.3 Recommended use of the chemical and restrictions on use Zinc ...