Electroless Nickel Part B MSDS

Electroless Nickel Part B MSDS

                                                                                             CASWELL INC

Safety Data Sheet
Electroless Nickel Part B
SECTION 1: Identification

1.1   Product identifier

      Product name                            Electroless Nickel Part B

      Product number                          ELECB
      Brand                                   Caswell

1.2   Other means of identification
      Electroless Cobalt Part B
      Electroless Nickel/Cobalt Part B

1.4   Supplier's details

      Name                                    Caswell Inc
      Address                                 7696 Route 31
                                              Lyons NY 14489
                                              USA

      Telephone                               315 946 1213
      Fax                                     315 946 4456
      email                                   sales@caswellplating.com

1.5   Emergency phone number(s)

                                              Office Hours (9-4ET): 315 946 1213
                                              24 Hour: CHEMTEL US# 1-800-255-3924                   Intl# +01-813-248-0585

SECTION 2: Hazard identification

2.1   Classification of the substance or mixture

      Not a hazardous substance or mixture.

2.2   GHS label elements, including precautionary statements

      Not a hazardous substance or mixture.

2.3   Other hazards which do not result in classification

      Not a hazardous substance or mixture.

                                                  Version: 1.1, Supersedes: 1.2, Date of issue: 2020-01-27, Printed on: 2020-01-27, p. 1 of 6
Safety Data Sheet
Electroless Nickel Part B

SECTION 3: Composition/information on ingredients

3.1   Substances

      Hazardous components

      1. OTHER NON-REPORTABLE INGREDIENTS
      Concentration               74 - 74 %

      2. Sodium hypophosphite
      Concentration                           25 - 25 %
      CAS no.                                 7681-53-0

      3. Ammonium hydroxide solution (5 - 10% NH3)
      Concentration                     1-1%
      EC no.                            215-647-6
      CAS no.                           1336-21-6
      Index no.                         007-001-01-2

      Trade secret statement (OSHA 1910.1200(i))
      Specific chemical names and formulas have been omitted as a trade secret under OSHA 1910.1200.

SECTION 4: First-aid measures

4.1   Description of necessary first-aid measures

      General advice                          Never give anything by mouth to an unconscious person. IF exposed or
                                              concerned: Get medical advice/attention

      If inhaled                              Assure fresh air breathing. Allow the victim to rest.

      In case of skin contact                 Remove affected clothing and wash all exposed skin area with mild soap and
                                              water, followed by warm water rinse.

      In case of eye contact                  Rinse immediately with plenty of water. Obtain medical attention if pain,
                                              blinking or redness persist.

      If swallowed                            Rinse mouth. Do NOT induce vomiting. Obtain emergency medical attention.

      Personal protective equipment for first-aid responders
                                              None required

SECTION 5: Fire-fighting measures

5.1   Suitable extinguishing media
      Foam. Dry powder. Carbon dioxide. Water spray. Sand.

5.3   Special protective actions for fire-fighters
      Use water spray or fog for cooling exposed containers. Exercise caution when fighting any chemical fire. Avoid
      (reject) fire-fighting water to enter environment. Do not enter fire area without proper protective equipment, including
      respiratory protection.


                                                  Version: 1.1, Supersedes: 1.2, Date of issue: 2020-01-27, Printed on: 2020-01-27, p. 2 of 6
Safety Data Sheet
Electroless Nickel Part B
SECTION 6: Accidental release measures

6.1   Personal precautions, protective equipment and emergency procedures
      Use chemically protective clothing.

6.2   Environmental precautions
      Prevent entry to sewers and public waters. Notify authorities if liquid enters sewers or public waters.

6.3   Methods and materials for containment and cleaning up
      Soak up with inert absorbent material and dispose of as hazardous waste. Keep in suitable, closed containers for
      disposal.

SECTION 7: Handling and storage

7.1   Precautions for safe handling
      Wash hands and other exposed areas with mild soap and water before eating, drinking or smoking and when
      leaving work. Provide good ventilation in process area to prevent formation of vapour. Do not handle until all safety
      precautions have been read and understood. Obtain special instructions before use.

7.2   Conditions for safe storage, including any incompatibilities
      Keep only in the original container in a cool, well ventilated place away from : incompatible materials. Keep
      container closed when not in use. Incompatible products: Oxidizing agent. Strong acids.

SECTION 8: Exposure controls/personal protection

8.2   Appropriate engineering controls
      Emergency eye wash fountains and safety showers should be available in the immediate vicinity of any potential
      exposure.

8.3   Individual protection measures, such as personal protective equipment (PPE)

      Eye/face protection
      Chemical goggles or safety glasses.

      Skin protection
      Wear protective gloves.

      Body protection
      Choose body protection in relation to its type, to the concentration and amount of dangerous substances, and to the
      specific work-place., The type of protective equipment must be selected according to the concentration and amount
      of the dangerous substance at the specific workplace.

      Respiratory protection
      Wear appropriate mask.

SECTION 9: Physical and chemical properties

      Information on basic physical and chemical properties

      Appearance/form (physical state, color, etc.)                   Clear Liquid
      Odor                                                            Strong Ammonia Odor
      Odor threshold
      pH                                                              5.5


                                                  Version: 1.1, Supersedes: 1.2, Date of issue: 2020-01-27, Printed on: 2020-01-27, p. 3 of 6
Safety Data Sheet
Electroless Nickel Part B
     Melting point/freezing point
     Initial boiling point and boiling range                       212 deg F
     Flash point
     Evaporation rate
     Flammability (solid, gas)
     Upper/lower flammability limits
     Vapor pressure
     Vapor density
     Relative density                                              1.18
     Solubility(ies)                                               Water
     Partition coefficient: n-octanol/water
     Auto-ignition temperature
     Decomposition temperature
     Viscosity
     Explosive properties
     Oxidizing properties

SECTION 10: Stability and reactivity

10.1 Reactivity
     None

10.2 Chemical stability
     Not Established

10.3 Possibility of hazardous reactions
     Not Established

10.4 Conditions to avoid
     Extremely high or low temperatures.

10.5 Incompatible materials
     Strong Acids. Strong Bases.

10.6 Hazardous decomposition products
     None

SECTION 11: Toxicological information

     Information on toxicological effects

     Acute toxicity
     Sodium Hypophosphite: Oral LD50: 7640 mg/kg

     Skin corrosion/irritation
     Not Classified

     Serious eye damage/irritation
     Not Classified

     Respiratory or skin sensitization
     Not Classified

     Germ cell mutagenicity

                                               Version: 1.1, Supersedes: 1.2, Date of issue: 2020-01-27, Printed on: 2020-01-27, p. 4 of 6
Safety Data Sheet
Electroless Nickel Part B
    Not classified

    Carcinogenicity
    Not classified

    Reproductive toxicity
    Not classified

    STOT-single exposure
    Not classified

    STOT-repeated exposure
    Not classified

SECTION 12: Ecological information

    Toxicity
    Not Established

    Persistence and degradability
    Not Established

    Bioaccumulative potential
    Not Established

    Mobility in soil
    Not Established

    Results of PBT and vPvB assessment
    Not Established

    Other adverse effects
    Avoid release to the environment.

SECTION 13: Disposal considerations

    Disposal of the product
    Dispose in a safe manner in accordance with local/national regulations. Dispose of contents/container to comply
    with local, state and federal regulations.

    Disposal of contaminated packaging
    Dispose in a safe manner in accordance with local/national regulations. Dispose of contents/container to comply
    with local, state and federal regulations.

    Waste treatment
    Avoid release to the environment.

SECTION 14: Transport information

    DOT (US)
    Not dangerous goods

    IMDG
    Not dangerous goods

                                              Version: 1.1, Supersedes: 1.2, Date of issue: 2020-01-27, Printed on: 2020-01-27, p. 5 of 6
Safety Data Sheet
Electroless Nickel Part B

      IATA
      Not dangerous goods

SECTION 15: Regulatory information

15.1 Safety, health and environmental regulations specific for the product in question
      Massachusetts Right To Know Components
      Chemical name: Ammonium hydroxide
      CAS number: 1336-21-6
      New Jersey Right To Know Components
      Common name: AMMONIUM HYDROXIDE
      CAS number: 1336-21-6
      Pennsylvania Right To Know Components
      Chemical name: Ammonium hydroxide
      CAS number: 1336-21-6

      HMIS Rating

              Electroless Nickel Part B
        HEALTH                             1
        FLAMMABILITY                       0
        PHYSICAL HAZARD                    0
        PERSONAL PROTECTION               C


      NFPA Rating




SECTION 16: Other information

16.1 Further information/disclaimer
     DISCLAIMER: The information above is believed to be accurate and represents the best information currently
     available to us. However, we make no warranty of merchantability or any other warranty, express or implied, with
     respect to such information, and we assume no liability resulting from its use. Users should make their own
     investigation to determine the suitability of information for their particular purposes. In no event shall Caswell Inc be
     liable for any claims, losses, or damages of any third party or for lost profits or any special, indirect, incidental,
     consequential or exemplary damages, whatsoever arising, even if Caswell Inc has been advised of the possibility of
     such damages.




                                                  Version: 1.1, Supersedes: 1.2, Date of issue: 2020-01-27, Printed on: 2020-01-27, p. 6 of 6

    • Related Articles

    • PTFE Electroless Nickel Part B MSDS

      PTFE Electroless Nickel Part B MSDS
    • Electroless Nickel Part C MSDS

      CASWELL INC Safety Data Sheet Electroless Nickel Part C SECTION 1: Identification 1.1 Product identifier Product name Electroless Nickel Part C Product number ELECC Brand Caswell 1.2 Other means of identification Electroless Cobalt Part C Electroless ...
    • Electroless Nickel Part A MSDS

      CASWELL INC Safety Data Sheet Electroless Nickel Plating Solution Part A SECTION 1: Identification 1.1 Product identifier Product name Electroless Nickel Plating Solution Part A Product number ELECA Brand Caswell 1.4 Supplier's details Name Caswell ...
    • B9 MSDS

      Metalx Specialty Products, Inc. B-9 Nickel Stripper, B-929, B-913, B-9 Plus, B-9 Nickel-Iron SDS Number: FP100 Revision Date: 5/15/2015 Page 1 of 7 1 PRODUCT AND COMPANY IDENTIFICATION Manufacturer Metalx Specialty Products, Inc 1333 Virginia St. ...
    • PTFE Electroless Nickel Part A MSDS

      PTFE Electroless Nickel Part A MSDS