Gas Tank Sealer Part A MSDS

Gas Tank Sealer Part A MSDS

                                                                                   CASWELL INC

Safety Data Sheet
Gas Tank Sealer Part A
SECTION 1: Identification

1.1   Product identifier

      Product name                          Gas Tank Sealer Part A

      Product number                        GTSA
      Brand                                 Caswell
      Substance name                        Epoxy resin
      CAS no.                               28064-14-4

1.2   Other means of identification
      Dragon's Blood, Black Magic, Petrol Blue, Battleship Grey, Royal Blue

1.4   Supplier's details

      Name                                  Caswell Inc
      Address                               7696 Route 31
                                            Lyons, NY 14489
                                            USA

      Telephone                             315 946 1213
      Fax                                   315 946 4456
      email                                 sales@caswellplating.com

1.5   Emergency phone number(s)

                                            Office Hours (9-4ET): 315 946 1213
                                            24 Hour: CHEMTEL US# 1-800-255-3924           Intl# +01-813-248-0585

SECTION 2: Hazard identification

2.1   Classification of the substance or mixture
      - Skin corrosion/irritation (chapter 3.2), Cat. 2
      - Eye damage/irritation (chapter 3.3), Cat. 2A
      - Sensitization, skin (chapter 3.4), Cat. 1
      - Hazardous to the aquatic environment - long-term hazard (chapter 4.1), Cat. 2

2.2   GHS label elements, including precautionary statements

      Pictogram


                                                                                  Version: 1.0, Date of issue: 2017-03-10, p. 1 of 8
Safety Data Sheet
Gas Tank Sealer Part A




      Signal word                        Warning

      Hazard statement(s)
      H315                               Causes skin irritation
      H319                               Causes serious eye irritation
      H317                               May cause an allergic skin reaction
      H411                               Toxic to aquatic life with long lasting effects

      Precautionary statement(s)
      P264                               Wash … thoroughly after handling.
      P280                               Wear protective gloves/protective clothing/eye protection/face protection.
      P302+P352                          IF ON SKIN: Wash with plenty of water/...
      P321                               Specific treatment (see … on this label).
      P332+P313                          If skin irritation occurs: Get medical advice/attention.
      P362+P364                          Take off contaminated clothing and wash it before reuse.
      P305+P351+P338                     IF IN EYES: Rinse cautiously with water for several minutes. Remove
                                         contact lenses if present and easy to do. Continue rinsing.
      P337+P313                          If eye irritation persists: Get medical advice/attention.
      P261                               Avoid breathing dust/fume/gas/mist/vapours/spray.
      P272                               Contaminated work clothing should not be allowed out of the workplace.
      P333+P313                          If skin irritation or a rash occurs: Get medical advice/attention.
      P501                               Dispose of contents/container to …
      P273                               Avoid release to the environment.
      P391                               Collect spillage.

SECTION 3: Composition/information on ingredients

3.1   Substances
      Substance name                     Epoxy resin
      CAS no.                            28064-14-4
      Formula                            C10H12O3
      Other names / synonyms             Phenol, polymer with formaldehyde, glycidyl ether; Epoxy resin

SECTION 4: First-aid measures

4.1   Description of necessary first-aid measures

      If inhaled                         Remove victim to fresh air and keep at rest in a position comfortable for
                                         breathing.
                                         If not breathing, if breathing is irregular or if respiratory arrest occurs, provide
                                         artificial respiration or oxygen by trained personnel. It may be dangerous to
                                         the
                                         person providing aid to give mouth-to-mouth resuscitation. Get medical
                                         attention if
                                         adverse health effects persist or are severe. If unconscious, place in
                                         recovery
                                         position and get medical attention immediately. Maintain an open airway.
                                         Loosen
                                         tight clothing such as a collar, tie, belt or waistband.

                                                                                  Version: 1.0, Date of issue: 2017-03-10, p. 2 of 8
Safety Data Sheet
Gas Tank Sealer Part A

      In case of skin contact                 Wash with plenty of soap and water. Remove contaminated clothing and
                                              shoes.
                                              Wash contaminated clothing thoroughly with water before removing it, or
                                              wear
                                              gloves. Continue to rinse for at least 10 minutes. Get medical attention. In
                                              the
                                              event of any complaints or symptoms, avoid further exposure. Wash
                                              clothing
                                              before reuse. Clean shoes thoroughly before reuse.

      In case of eye contact                  Immediately flush eyes with plenty of water, occasionally lifting the upper and
                                              lower
                                              eyelids. Check for and remove any contact lenses. Continue to rinse for at
                                              least 10
                                              minutes. Get medical attention.

      If swallowed                            Wash out mouth with water. Remove dentures if any. Remove victim to
                                              fresh air
                                              and keep at rest in a position comfortable for breathing. If material has been
                                              swallowed and the exposed person is conscious, give small quantities of
                                              water to
                                              drink. Stop if the exposed person feels sick as vomiting may be dangerous.
                                              Do not
                                              induce vomiting unless directed to do so by medical personnel. If vomiting
                                              occurs,
                                              the head should be kept low so that vomit does not enter the lungs. Get
                                              medical
                                              attention if adverse health effects persist or are severe. Never give anything
                                              by
                                              mouth to an unconscious person. If unconscious, place in recovery position
                                              and get
                                              medical attention immediately. Maintain an open airway. Loosen tight
                                              clothing such
                                              as a collar, tie, belt or waistband

      Personal protective equipment for first-aid responders
                                              See section 8

4.3   Indication of immediate medical attention and special treatment needed, if necessary
      No specific treatment. Treat symptomatically. Call medical doctor or poison control
      center immediately if large quantities have been ingested.

SECTION 5: Fire-fighting measures

5.1   Suitable extinguishing media
      Use an extinguishing agent suitable for the surrounding fire

5.2   Specific hazards arising from the chemical
      In a fire or if heated, a pressure increase will occur and the container may burst.
      This material is toxic to aquatic life with long lasting effects. Fire water
      contaminated with this material must be contained and prevented from being
      discharged to any waterway, sewer or drain.


                                                                                      Version: 1.0, Date of issue: 2017-03-10, p. 3 of 8
Safety Data Sheet
Gas Tank Sealer Part A
SECTION 6: Accidental release measures

6.3   Methods and materials for containment and cleaning up
      Stop leak if without risk. Move containers from spill area. Approach release from
      upwind. Prevent entry into sewers, water courses, basements or confined areas.
      Wash spillages into an effluent treatment plant or proceed as follows. Contain and
      collect spillage with non-combustible, absorbent material e.g. sand, earth,
      vermiculite or diatomaceous earth and place in container for disposal according to
      local regulations (see Section 13). Dispose of via a licensed waste disposal
      contractor. Contaminated absorbent material may pose the same hazard as the
      spilled product. Note: see Section 1 for emergency contact information and Section
      13 for waste disposal.

SECTION 7: Handling and storage

7.1   Precautions for safe handling
      Put on appropriate personal protective equipment (see Section 8). Persons with a
      history of skin sensitization problems should not be employed in any process in
      which this product is used. Do not get in eyes or on skin or clothing. Do not ingest.
      Avoid breathing vapor or mist. Avoid release to the environment. Keep in the
      original container or an approved alternative made from a compatible material, kept
      tightly closed when not in use. Empty containers retain product residue and can be
      hazardous. Do not reuse container.

SECTION 8: Exposure controls/personal protection

8.2   Appropriate engineering controls
      No special ventilation requirements. Good general ventilation should be sufficient to
      control worker exposure to airborne contaminants. If this product contains
      ingredients with exposure limits, use process enclosures, local exhaust ventilation or
      other engineering controls to keep worker exposure below any recommended or
      statutory limits.

8.3   Individual protection measures, such as personal protective equipment (PPE)

      Pictograms




      Eye/face protection
      Safety eyewear complying with an approved standard should be used when a risk
      assessment indicates this is necessary to avoid exposure to liquid splashes, mists,
      gases or dusts. If contact is possible, the following protection should be worn,
      unless the assessment indicates a higher degree of protection: chemical splash
      goggles.

      Skin protection
      Chemical-resistant, impervious gloves complying with an approved standard should
      be worn at all times when handling chemical products if a risk assessment indicates
      this is necessary. Considering the parameters specified by the glove manufacturer,
      check during use that the gloves are still retaining their protective properties. It
      should be noted that the time to breakthrough for any glove material may be


                                                                                    Version: 1.0, Date of issue: 2017-03-10, p. 4 of 8
Safety Data Sheet
Gas Tank Sealer Part A
     different for different glove manufacturers. In the case of mixtures, consisting of
     several substances, the protection time of the gloves cannot be accurately
     estimated. > 8 hours (breakthrough time): butyl rubber, Ethyl Vinyl Alcohol
     Laminate (EVAL)

     Body protection
     Personal protective equipment for the body should be selected based on the task
     being performed and the risks involved and should be approved by a specialist
     before handling this product.

     Respiratory protection
     Use a properly fitted, air-purifying or air-fed respirator complying with an approved
     standard if a risk assessment indicates this is necessary. Respirator selection must
     be based on known or anticipated exposure levels, the hazards of the product and
     the safe working limits of the selected respirator

     Environmental exposure controls
     Emissions from ventilation or work process equipment should be checked to ensure
     they comply with the requirements of environmental protection legislation. In some
     cases, fume scrubbers, filters or engineering modifications to the process
     equipment will be necessary to reduce emissions to acceptable levels.

SECTION 9: Physical and chemical properties

     Information on basic physical and chemical properties

     Appearance/form (physical state, color, etc.)                Gray Liquid
     Odor                                                         Slight
     Odor threshold                                               Not available.
     pH                                                           6
     Melting point/freezing point                                 Not available.
     Initial boiling point and boiling range                      >200 deg C
     Flash point                                                  Closed Cup > 200 deg C
     Evaporation rate                                             Not available.
     Flammability (solid, gas)                                    Not available.
     Upper/lower flammability limits                              Not available.
     Vapor pressure                                               <0.0001 kPa
     Vapor density                                                Not available.
     Relative density                                             Not available.
     Solubility(ies)                                              insoluble
     Partition coefficient: n-octanol/water                       Not available.
     Auto-ignition temperature                                    Not available.
     Decomposition temperature                                    > 200 deg C
     Viscosity                                                    Not available.
     Explosive properties                                         Not available.
     Oxidizing properties                                         Not available.

     Other safety information
     Product does not contain Volatile Organic Compounds

SECTION 10: Stability and reactivity

10.1 Reactivity
     Not available.

                                                                                     Version: 1.0, Date of issue: 2017-03-10, p. 5 of 8
Safety Data Sheet
Gas Tank Sealer Part A

10.2 Chemical stability
     Stable

10.3 Possibility of hazardous reactions
     Not available.

10.4 Conditions to avoid
     Not available.

10.5 Incompatible materials
     Not available.

10.6 Hazardous decomposition products
     Not available.

SECTION 11: Toxicological information

     Information on toxicological effects

     Acute toxicity
     Bisphenol F epoxy resin
     LD50 Dermal
     Rat - Male, Female >2000 mg/kg

     Skin corrosion/irritation
     Bisphenol F epoxy resin
     OECD 405 Acute Eye Irritation/
     Corrosion Rabbit Eyes - Non-irritant.

     Carcinogenicity
     None

     Reproductive toxicity
     None

     STOT-single exposure
     Not Available

     STOT-repeated exposure
     Not Available

     Aspiration hazard
     Not Available

SECTION 12: Ecological information

     Toxicity
     Bisphenol F epoxy resin
     OECD 201 Alga, Growth Inhibition Test
     Acute EC50 72 hours Static
     Algae
     1.8 mg/l


                                             Version: 1.0, Date of issue: 2017-03-10, p. 6 of 8
Safety Data Sheet
Gas Tank Sealer Part A
SECTION 13: Disposal considerations

      Disposal of the product
      The generation of waste should be avoided or minimized wherever possible.
      Disposal of this product, solutions and any by-products should at all times comply
      with the requirements of environmental protection and waste disposal legislation
      and any regional local authority requirements. Dispose of surplus and non-
      recyclable products via a licensed waste disposal contractor. Waste should not be
      disposed of untreated to the sewer unless fully compliant with the requirements of
      all authorities with jurisdiction. Waste packaging should be recycled. Incineration or
      landfill should only be considered when recycling is not feasible. This material and
      its container must be disposed of in a safe way. Care should be taken when
      handling emptied containers that have not been cleaned or rinsed out. Empty
      containers or liners may retain some product residues. Avoid dispersal of spilled
      material and runoff and contact with soil, waterways, drains and sewers.

SECTION 14: Transport information

      DOT (US)
      Not dangerous goods

      IMDG
      Not dangerous goods

      IATA
      Not dangerous goods

SECTION 15: Regulatory information

      HMIS Rating

                     Epoxy resin
        HEALTH                            2
        FLAMMABILITY                      1
        PHYSICAL HAZARD                   0
        PERSONAL PROTECTION


      NFPA Rating




SECTION 16: Other information

16.1 Further information/disclaimer
     DISCLAIMER: The information above is believed to be accurate and represents the best information currently
     available to us. However, we make no warranty of merchantability or any other warranty, express or implied, with
     respect to such information, and we assume no liability resulting from its use. Users should make their own

                                                                                    Version: 1.0, Date of issue: 2017-03-10, p. 7 of 8
Safety Data Sheet
Gas Tank Sealer Part A
    investigation to determine the suitability of information for their particular purposes. In no event shall Caswell Inc be
    liable for any claims, losses, or damages of any third party or for lost profits or any special, indirect, incidental,
    consequential or exemplary damages, whatsoever arising, even if Caswell Inc has been advised of the possibility of
    such damages.




                                                                                    Version: 1.0, Date of issue: 2017-03-10, p. 8 of 8

    • Related Articles

    • Gas Tank Sealer Part B MSDS

      CASWELL INC Safety Data Sheet Gas Tank Sealer Part B SECTION 1: Identification 1.1 Product identifier Product name Gas Tank Sealer Part B Product number GTSB Brand Caswell 1.2 Other means of identification Dragon's Blood, Black Magic, Petrol Blue, ...
    • Gas Tank Sealer Instructions

      7696 Route 31 Lyons NY 14489 USA http://www.caswellplating.com 315-946-1213 Fax 315-946-4456 GAS TANK SEALER Application Instructions READ THIS COMPLETE INSTRUCTION SHEET BEFORE STARTING Preparation 1. All traces of oil and gasoline should first be ...
    • Can You Tint Gas Tank Sealer?

      Q: Can you tint your Gas Tank Sealer? A: Yes you can. You can use a tint designed for use with an oil based paint.
    • Does your gas tank sealer work on plastic and fiberglass tanks?

      Yes. To apply gas tank sealer on plastic or fiberglass tanks, take a handful of drywall screws and shake them around inside the tank for a few minutes. This roughs up the surface of the tank, providing best adhesion for the sealer. Follow the mixing ...
    • Gas Tank Stripper No Methylene Chloride SDS

      CASWELL INC Safety Data Sheet Gas Tank Stripper No Methylene Chloride SECTION 1: Identification 1.1 Product identifier Product name Gas Tank Stripper No Methylene Chloride Product number GSTRIPNM Brand Caswell 1.3 Recommended use of the chemical and ...