How Long Will My Plate Last?
That depends on how long you plate your part for. The longer you plate it, the longer the plate will last. All our plating kits use the same chemicals and processes as the plating shops that plated your parts originally. You can expect the same or better durability than the original plate.
Related Articles
How much will the Plug N' Plate solutions plate?
At an average thickness the kits will plate approximately: 4oz Gold - 0.5 - 1 sq ft 4oz Silver - 1 sq ft 8oz Nickel - 2 sq ft 8oz Copper - 2 sq ft 8oz Copy Chrome - 2 sq ft 8oz Bronze - 2 sq ft 8oz Tin - 2 sq ft 4oz Brass - 1 sq ft
My Plug N Plate Kit Doesn't Plate
If your Plug N Plate® kit doesn't plate, check the following things: Check your connections are correct and tight. The black alligator clip should be on the part being plated, and the wand should be on the red banana plug and tight. Check the bandage ...
gp plate SDS
CASWELL INC Safety Data Sheet GP Plate SECTION 1: Identification 1.1 Product identifier Product name GP Plate Product number GPPL Brand Caswell Substance name LEAD POWDER CAS no. 7439-92-1 1.3 Recommended use of the chemical and restrictions on use ...
Plug N Plate® Kit Instructions
Plug N’ Plate® Brush Plating System I am a watchmaker in Scottsdale, Arizona and I specialize in restorations of fine antique watches and clocks. I was recently commissioned to restore a one-of-a-kind French clock, Circa. 1860 which was ornamented ...
Copy Cad/Zinc Plating Kit FAQ
COPY/CAD FAQ Why is my bath cloudy ? Why are my parts coming out dull ? What type of filter should I use ? My parts come out shiney but have a white film/haze on them What should my PH be and how do I adjust it ? Where should I set my Voltage ? Do I ...