How can I do Titanium Anodizing?
For reference only – Caswell Inc. does not support this
procedure.

Any electrolyte will do: phosphoric, coca-cola, sulfuric

Colors are achieved by varying oxide thickness.

Colors are achieved thru refraction of light on titanium surface. The color
changes with the voltage rather than amperage. Clean parts in 25%-30% nitric
with 2-4 oz/gal HF


              1-8 volts                          yellow
              9-12 volts                         brown
              13-20 volts                        maroon
              21-25 volts                        blue
              26-35 volts                        green
              36-45 volts                        gold
              46-50 volts                        rose
              70 volts                           purple/fusia

    • Related Articles

    • Titanium Anodizing Powder SDS

      CASWELL INC Safety Data Sheet Titanium Anodizing Powder SECTION 1: Identification 1.1 Product identifier Product name Titanium Anodizing Powder Product number TAP Brand Caswell 1.4 Supplier's details Name Caswell Inc Address 7696 Route 31 Lyons, NY ...
    • LCD Anodizing Instructions

      CASWELL LCD ANODIZING SYSTEM CASWELL INC 7696 ROUTE 31, LYONS NY 14489 USA WWW.CASWELLPLATING.COM SALES@CASWELLPLATING.COM 855-CASWELL © 2020 CASWELL INC CASWELL’S LCD ANODIZING SYSTEM A revolution in Small Scale Anodizing! Provides a durable ...
    • BLACK ANODIZING DYE MSDS

      BLACK ANODIZING DYE MSDS
    • What is LCD Anodizing?

      LCD stands for Low Current Density and is a revolutionary way for amateur anodizers with small anodizing lines to get consistently good results. LCD uses a low and slow method of anodizing. More technical details about LCD are available by reading ...
    • DEEP RED ANODIZING DYE MSDS

      CASWELL INC Safety Data Sheet Deep Red Dye SECTION 1: Identification 1.1 Product identifier Product name Deep Red Dye Product number DYEDR Brand Caswell 1.3 Recommended use of the chemical and restrictions on use Dye for aluminum 1.4 Supplier's ...