| DYES |
OPTIMUM Ph |
| RED BORDEAUX |
6 |
| YELLOW 4A |
6 |
| BLUE 4 A |
6 |
| VIOLET 3D |
6 |
| BLACK HBL |
5.5 |
| GREEN SCG |
6.6 |
| GOLD S |
6 |
| TURQUOISE |
5.5 |
| OLIVE DRAB |
7.5 |
| GOLDEN ORANGE |
7 |
| GREY BL |
5.5 |
| BROWN GL |
6.5 |
| TEAL |
5.5 |
| ELECTRIC BLUE |
6 |
| COPPER BF |
7 |
| FLOURESCENT PINK |
|
| BRONZE |
5.5 |
| DEEP RED |
5.5 |
| FLOURESCENT YELLOW |
6 |
| GREEN AEN |
6 |
| VIOLET DS |
6 |
| GREY NLN |
5.5 |
| YELLOW 3GL |
6 |
| BROWN BL |
6.5 |
| FAST BLUE |
5.5 |
| ORANGE 3A |
6 |