What's the difference between Extreme Chrome And Super Chrome
Q: Whats the difference between EXTREME CHROME & SUPER CHROME? Is either a single stage spray?
A: There's no such thing as single stage chrome powder if you intend for the parts to be used outdoors. Other companys market a single stage chrome, but fail to tell you that they're only single stage if the parts don't ever see the elements. Metal flake in the metallic powders will corrode and dull over time if not clearcoated.
Extreme Chrome is cheaper, and has a higher gloss rating. Most people prefer it over Super Chrome.
Related Articles
chrome crystals
CASWELL INC Safety Data Sheet Chrome Crystals SECTION 1: Identification 1.1 Product identifier Product name Chrome Crystals Product number C15C Brand Caswell Substance name CHROMIUM TRIOXIDE EC no. 215-607-8 1.3 Recommended use of the chemical and ...
Decorative Chrome Crystals MSDS
If you have purchased this product and need an MSDS, please e-mail us for the password.
Hard Chrome Crystals MSDS
If you have purchased this product and need an MSDS, please e-mail us for the password.
Super Stripper MSDS
CASWELL INC Safety Data Sheet Super Stripper SECTION 1: Identification 1.1 Product identifier Product name Super Stripper Product number SS1012 1.3 Recommended use of the chemical and restrictions on use Liquid Powder Coating Stripper 1.4 Supplier’s ...
What's the difference between Hard Chrome and Decorative Chrome?
Decorative chrome is a thin plate of chrome that is applied for reasons of appearance. Most chroming applications are decorative chrome applications. Hard chrome is a thick layer of chrome that is used to rebuild items in industrial applications such ...