Decorative chrome is a thin plate of chrome that is applied for reasons of appearance. Most chroming applications are decorative chrome applications. Hard chrome is a thick layer of chrome that is use...
Large scale chrome plating shops use a Triple Chrome process, which consists of copper plating, nickel plating, then chrome plating. Our Triple Chrome Plating kit duplicates this process on a small sc...
Yes! But if you follow our instructions, and use the supplied fume control system and some common sense, you can chrome plate all day and night without any problems....
Triple Chrome is a real chrome plate and is applied in three steps: Copper, Nickel, then Chrome. It uses chromic acid, which is a dangerous chemical. Triple Chrome now includes Flash Copper, which all...