Q: What is the phosphorous level in your Electroless Nickel and Krome Kits? A: It's a mid phosphorous formula, 5-9%....
If you buy our Jumbo Electroless Nickel, or Electroless Krome kits, the cost of the plating works out to approx $0.50 per square inch, when plated at 1/1000 After the initial purchase of the kit, buyi...
The solution needs be heated to 190°F, so it can be more inconvenient to use. The nickel is depleted from the solution, not anodes, so it will need to be replenished constantly and is more expensive ...
Electroless plating requires no power source. The metal is deposited on the part using a complex chemical reaction, rather than being forced onto the part by a power source. Electroless plating usuall...
Firstly, you don't have to spend money on a power source and you don't have to make any electrical calculations or connections. You don't have to worry about anode placement, because the solution will...