  • What's the difference between Extreme Chrome And Super Chrome

    Q: Whats the difference between EXTREME CHROME & SUPER CHROME? Is either a single stage spray? A: There's no such thing as single stage chrome powder if you intend for the parts to be used outdoors. O...

  • Powder Coat Coverage

    Q: Approximately how much coverage can I get per pound of powder coating material? A: One pound of powder will cover approx 50-100 sq ft. -- Caswell Inc. 7696 Route 31, Lyons NY 14489 USA P: 315 946 1...