Q: Can you tint your Gas Tank Sealer? A: Yes you can. You can use a tint designed for use with an oil based paint....
Yes. To apply gas tank sealer on plastic or fiberglass tanks, take a handful of drywall screws and shake them around inside the tank for a few minutes. This roughs up the surface of the tank, providin...