Does your gas tank sealer work on plastic and fiberglass tanks?
Yes.
To apply gas tank sealer on plastic or fiberglass tanks, take a handful of drywall screws and shake them around inside the tank for a few minutes. This roughs up the surface of the tank, providing best adhesion for the sealer. Follow the mixing and application directions that are printed on the product.
Related Articles
Gas Tank Sealer Instructions
7696 Route 31 Lyons NY 14489 USA http://www.caswellplating.com 315-946-1213 Fax 315-946-4456 GAS TANK SEALER Application Instructions READ THIS COMPLETE INSTRUCTION SHEET BEFORE STARTING Preparation 1. All traces of oil and gasoline should first be ...
Gas Tank Sealer Part B MSDS
CASWELL INC Safety Data Sheet Gas Tank Sealer Part B SECTION 1: Identification 1.1 Product identifier Product name Gas Tank Sealer Part B Product number GTSB Brand Caswell 1.2 Other means of identification Dragon's Blood, Black Magic, Petrol Blue, ...
Gas Tank Sealer Part A MSDS
CASWELL INC Safety Data Sheet Gas Tank Sealer Part A SECTION 1: Identification 1.1 Product identifier Product name Gas Tank Sealer Part A Product number GTSA Brand Caswell Substance name Epoxy resin CAS no. 28064-14-4 1.2 Other means of ...
Gas Tank Stripper No Methylene Chloride SDS
CASWELL INC Safety Data Sheet Gas Tank Stripper No Methylene Chloride SECTION 1: Identification 1.1 Product identifier Product name Gas Tank Stripper No Methylene Chloride Product number GSTRIPNM Brand Caswell 1.3 Recommended use of the chemical and ...
Can You Tint Gas Tank Sealer?
Q: Can you tint your Gas Tank Sealer? A: Yes you can. You can use a tint designed for use with an oil based paint.