Stripping Chrome From Emblems

Stripping Chrome From Emblems

To strip chrome from emblems using a wand (Plug N Plate), ensure the wand is on the negative terminal. Wrap a new bandage around the wand. Touch the positive lead to the part. Dip the wand in the stripper solution and briskly stroke it over the part. A yellow stain will appear on the bandage. This is the chrome coming off.

Under the chrome is a nickel plate. Chrome and nickel look very similar...in fact, many people believe that the chrome stripper is not working, when in fact the chrome has all been removed and they are now looking at the nickel. To ensure that all the chrome is off, simply change your wand bandage regularly until you don't see anymore yellow stain.

The nickel plate may now be gold plated. There's no need to "activate" this nickel plate before plating with gold.

    • Related Articles

    • chrome crystals

      CASWELL INC Safety Data Sheet Chrome Crystals SECTION 1: Identification 1.1 Product identifier Product name Chrome Crystals Product number C15C Brand Caswell Substance name CHROMIUM TRIOXIDE EC no. 215-607-8 1.3 Recommended use of the chemical and ...
    • Decorative Chrome Crystals MSDS

      If you have purchased this product and need an MSDS, please e-mail us for the password.
    • Hard Chrome Crystals MSDS

      If you have purchased this product and need an MSDS, please e-mail us for the password.
    • PROFFESIONAL GOLD PNP

      CASWELL Inc PROFESSIONAL GOLD PLATING INSTRUCTIONS BRUSH PLATING 3 Amp Constant Current Rectifier ! Constant current/voltage power control - Only $95.00 This new system has the latest technology for small plating and anodizing operations. Several of ...
    • What's the difference between Hard Chrome and Decorative Chrome?

      Decorative chrome is a thin plate of chrome that is applied for reasons of appearance. Most chroming applications are decorative chrome applications. Hard chrome is a thick layer of chrome that is used to rebuild items in industrial applications such ...